Light Link™ SLA resin for 3D printing is designed for printing Kynar® PVDF parts using low-cost consumer-grade SLA printers. Whether you want to print small PVDF parts with careful detail or large complex components, Light Link™ is up to the task. Our low-odor resin prints with ease and requires short exposure times and convenient post-processing methods. Light Link™ is formulated for low shrinkage and easy removal from the build plate. No matter the printing task at hand, Light Link™ delivers a quality result.
Light Link™ prints are a beautiful, glossy white color. These parts have scratch-resistant properties and almost invisible layer lines. Approaching the quality of injection molded parts Light Link™ prints are a cost-effective alternative without the mold expense. Easy print resin produces parts that clean up with standard post-processing procedures. Wash with IPA and post-cure with UV light, like all other 3D printed resins. There are no expensive printers, complex slicer settings, steep learning curves or extra accessories required to create beautiful Light Link™ parts.
Each bottle contains 1 kilogram of Light Link™ photopolymer resin. Always shake well before using and keep stored at 15-25 °C.
-
White Photopolymer Resin and Finished Parts
-
Invisible Layer Lines
-
High-Performance Prints
-
Excellent Tensile Strength
-
Moderate Impact Strength
-
Moderate Elongation
-
Scratch Resistant Prints
- Low Odor Resin
-
Compatible with Most Low-Cost SLA Printers
-
Shake the bottle vigorously for 60 – 120 seconds before use.
-
Allow the Light Link™ resin to rest for a few minutes after shaking to allow air bubbles to dissipate before adding to the vat.
-
Begin printing!
- The PVDF SLA Resin can be poured back into the bottle for reuse. Always use appropriate filtration methods when returning used PVDF SLA resin to the bottle to restrict cross-contamination and to exclude polymerized pieces of resin. For more information on handling the resin, see SDS and TDS.
-
Resin Vat Temperature: Heated vats are not required. Light Link™ resin prints using any vat. Print between 15 – 30 °C
-
Normal Layer Exposure Time: 5.0 – 9.5 seconds (7.0 seconds is generally recommended)
-
Bottom Layer Exposure Time: 30.0 – 55.0 seconds (45.0 seconds is generally recommended)
-
Post-Processing: Wash prints using 99% Isopropyl alcohol for 5 – 10 minutes. Let air dry. UV cure for 2-10 minutes (depending on the size of the print). For superior prints, wash prints with Isopropyl alcohol for 5 – 10 minutes and let air dry. Any post-processing techniques can be performed at this time.
-
Adhesion: To improve bottom layer adhesion, gently sand the build plate of the printer. Please consult with your specific SLA instruction manual before modifying the printer.
-
Container: Bottle
-
Net Weight: 1 kg
-
Wavelength: 385 – 405nm
-
FlashForge Hunter DLP Printer
-
Elegoo Saturn MSLA Printer
-
Elegoo Mars Series SLA Printers
-
Elegoo Series MSLA/SLA Printers
-
Phrozen Series MSLA/SLA/DLP printers
-
Anycubic Series MSLA/SLA/DLP Printers
Note: More printers will be added to the list as they are tested.